Rose's metal, Rose metal or Rose's alloy is a fusible alloy with a low melting point.
Rose's metal consists of 50% bismuth, 25–28% lead and 22–25% tin. Its melting point is between 94 and 98 °C (201 and 208 °F). The alloy does not appreciably contract or expand on solidification, this characteristic being a function of its bismuth percentage, but does slightly contract on cooling.
Rose's metal has several common uses:
It was discovered by the German chemist Valentin Rose the Elder, the grandfather of Heinrich Rose.
| Alloy | Melting point | Eutectic? | Bismuth % | Lead % | Tin % | Indium % | Cadmium % | Thallium % | Gallium % | Antimony % |
|---|---|---|---|---|---|---|---|---|---|---|
| Rose's metal | 98 °C (208 °F) | No | 50 | 25 | 25 | N/a | N/a | N/a | N/a | N/a |
| Cerrosafe | 74 °C (165 °F) | No | 42.5 | 37.7 | 11.3 | N/a | 8.5 | N/a | N/a | N/a |
| Wood's metal | 70 °C (158 °F) | Yes | 50 | 26.7 | 13.3 | N/a | 10 | N/a | N/a | N/a |
| Field's metal | 62 °C (144 °F) | Yes | 32.5 | N/a | 16.5 | 51 | N/a | N/a | N/a | N/a |
| Cerrolow 136 | 58 °C (136 °F) | Yes | 49 | 18 | 12 | 21 | N/a | N/a | N/a | N/a |
| Cerrolow 117 | 47.2 °C (117 °F) | Yes | 44.7 | 22.6 | 8.3 | 19.1 | 5.3 | N/a | N/a | N/a |
| Bi-Pb-Sn-Cd-In-Tl | 41.5 °C (107 °F) | Yes | 40.3 | 22.2 | 10.7 | 17.7 | 8.1 | 1.1 | N/a | N/a |
| Gallium | 29.8 °C (86 °F) | Pure metal | N/a | N/a | N/a | N/a | N/a | N/a | 100 | N/a |
| Galinstan | −19 °C (−2 °F) | No | <1.5 | N/a | 9.5–10.5 | 21–22 | N/a | N/a | 68–69 | <1.5 |